Home ProductsPrecious Metal Tester

KUT-681 Digital Portable Ultrasonic Flaw Detector, for metal weld crack, inclusion, pore defect inspection & composite thickness testing

KUT-681 Digital Portable Ultrasonic Flaw Detector, for metal weld crack, inclusion, pore defect inspection & composite thickness testing

    • KUT-681 Digital Portable Ultrasonic Flaw Detector, for metal weld crack, inclusion, pore defect inspection & composite thickness testing
    • KUT-681 Digital Portable Ultrasonic Flaw Detector, for metal weld crack, inclusion, pore defect inspection & composite thickness testing
    • KUT-681 Digital Portable Ultrasonic Flaw Detector, for metal weld crack, inclusion, pore defect inspection & composite thickness testing
    • KUT-681 Digital Portable Ultrasonic Flaw Detector, for metal weld crack, inclusion, pore defect inspection & composite thickness testing
    • KUT-681 Digital Portable Ultrasonic Flaw Detector, for metal weld crack, inclusion, pore defect inspection & composite thickness testing
    • KUT-681 Digital Portable Ultrasonic Flaw Detector, for metal weld crack, inclusion, pore defect inspection & composite thickness testing
  • KUT-681 Digital Portable Ultrasonic Flaw Detector, for metal weld crack, inclusion, pore defect inspection & composite thickness testing

    Product Details:

    Place of Origin: Dongguan, Guangdong
    Brand Name: HONTOTEST
    Certification: ISO,SGS
    Model Number: KUT-681

    Payment & Shipping Terms:

    Minimum Order Quantity: one set
    Price: negotiable
    Packaging Details: Wooden Box
    Delivery Time: 3-5 working days
    Payment Terms: L/C, D/A, D/P, T/T, Western Union,
    Supply Ability: 300 sets per month
    Contact Now
    Detailed Product Description
    Range: 0 To 15m, At Steel Velocity,transmit 30m Velocity: 100~ 15000m/s
    Pulse Repetition: 20~2000Hz Dynamic Range: ≥36dB
    Vertical Linearity: ≤2.5% Horizontal Linearity: ≤0.2%

    KUT-681 Digital Portable Ultrasonic Flaw Detector, for metal weld crack, inclusion, pore defect inspection & composite thickness testing

     

    Introduction:

     

    This instrument is a digital portable ultrasonic flaw detector for quickly, conveniently, damage-free and accurately to detect, locate, evaluate and diagnose various internal defects of the work piece (cracks, inclusions, pores, etc.). It can also be used for thickness detection and quality control for composite materials.

    The waveform can be saved in a standard file format, such as CSV

    Or Directly generate PDF report, BMP report by pressing the easy button

    For the advanced model, provide dedicated weld menu which allows to set the shape, groove, and real-time to defect weld flaw location according to the plate thickness and welding method

     

    Shape:

     

    • Ergonomic structural design, waterproof and oil-proof.

    • 360-degree rotating damping bracket and rubber sheath

    • High transparent strong aperture glass panel

     

    Display:

     

    • Full digital muti-color display, master-slave menu, clear guide

    • IPS (In-Plane Switching) ,no viewing angle, 640X480 high resolution

    • 60Hz display refresh rate, quickly displays small defect wave forms

    • High brightness display can be used under strong light.

    • 4 operating interface styles, and the LCD brightness can be set freely

    KUT-681 Digital Portable Ultrasonic Flaw Detector, for metal weld crack, inclusion, pore defect inspection & composite thickness testing

    KUT-681 Digital Portable Ultrasonic Flaw Detector, for metal weld crack, inclusion, pore defect inspection & composite thickness testing

     

    Real-time screenshot of all pages and flaw detection reports, and save them as BMP pictures to U disk, which can be set as color or grayscale pictures.

     

    • Export the flaw detection report as a PDF file and save it to a U disk for easy archiving and printing

    • All contents of the PDF file can be customized according to user needs.

    • BMP pictures and PDF files can be viewed on a computer or mobile phone

    KUT-681 Digital Portable Ultrasonic Flaw Detector, for metal weld crack, inclusion, pore defect inspection & composite thickness testing

     

    Functions:

     

    • Auto calibration: Automated calibration of probe zero offset, probe angle (K value) and material velocity

    • Peak Hold: Compare frozen peak waveforms to live A-Scans to easily interpret test results

    • Flaw Locating:Live display Sound-path, Projection (surface distance), Depth, Amplitude

    • Flaw sizing: Automatic flaw sizing using AVG or DAC, speeds reporting of defect acceptance or rejection.

    • Curved Surface Correction feature

    • DAC/AVG:The curve is automatically generated, and the sampling points can be compensated and corrected. The curve automatically floats with the gain, automatically expands with the detection distance, and automatically moves with the delay time. It can display the AVG curve of any aperture

    • AWS D1.1. Choosing this standard can reduce manual calculations and improve detection efficiency

    • Crack Height Measure function

    • Gate Magnify :spreading of the gate range over the entire screen width

    • Video Recording and playback

    • A Scan Freeze:Display freeze holds waveform and test distance data

    • Echo coding: display 1~9 echo display area in different colors, used to analyze the defect position

    • Peak mark: capture and mark the peak in real time

    • B Scan display feature. Intuitively display the defect shape and the detection result is more intuitive

    • Digital Readout and Trig. Function: Thickness/Depth can be displayed in digital readout when using a normal probe and Surface Distance and Depth are directly displayed when angle probe is in use

    • FFT spectrum analysis by calculate the echo waveform, to detect the frequency characteristics and damage degree of the current probe in real time

     

    Standard Package:

     

    Host 1PC

    Straight Probe 1PC

    Angle probe 1 PC

    Power Adaptor 1 PC

    Probe Connecting Cable 1 PC

    U disk 1 PC

    User Manual 1PC

    Instrument Case 1 PC

     

    Technical Parameter:

     

      Standard Advanced
    Range 0 to 15m, at steel velocity,transmit 30m 0 to 20m, at steel velocity,transmit 40m
    Velocity 100~ 15000m/s 100~20000m/s
    Pulse Repetition 20~2000Hz
    Dynamic range ≥36dB
    Vertical Linearity ≤2.5%
    Horizontal Linearity ≤0.2%
    Resolving Power >40dB(5P14in steel)
    Sensitivity Leavings >65dB(2.5MHzФ20mm)for Deep 200mmФ2 flat-bottomed hole,wave H50%)
    Noise ≤10%
    Channel files 500 files to store calibration setups and probe parameter
    Report files 1000 reports in PDF format
    Display IPS display 60Hz 60Hz display refresh rate, resolution 640X480
    Reject (suppression) 0~80% of full screen height
    Probe Type straight probe, angle probe, dual probe, penetrating etc.
    Gate Monitors Two independent gates controllable over entire sweep range
    trigger Peak trigger,Edge trigger
    Alarms Threshold positive/negative with LED Flash
    Power supply AC Mains 100-240 VAC, 50-60 Hz
      Lithium-ion Battery(DC)9V, more than 12 H working hours

     

    Auxiliary function

    Screen capture, video recording and playback, B-scan, DAC, AVG, AWS data analysis software
    Advanced function   Weld diagram, probe frequency detection

     

    Video Recorder

    10 video files, each video file can be up to 5 minutes long, 30 frames per second. save in U-disk for mass memory(no limit for duration)
    Dimension 230×157×52(mm)
    Weight 1. 12kg
    Environment humidity (- 10~50)℃
    Relative humidity (20~95)%RH
    Protection level IP65 IP67

     

    Pulse Energy

    Pulse amplitude: 100V, 200V, 250V, 300V, 350V, 400V, 450V, 500V graded selection, suitable for a wide range of probes
    Pulse Width from 0.1µs to 0.5 µs to match the probes with different frequency
    Probe Damping 50Ω, 150Ω, 300Ω and 400Ω are optional to meet different working requirements of sensitivity and resolution
    Scan speed 16 digit AD Converter at the sampling speed of 320 MHz
    Rectification Positive Hal fwave, Negative Half wave, Full wave and RF
    Bandwidth 0.1-20MHz,amplifier bandpass and narrow bandpass
    Gain 110dB(0.1dB;1dB;2dB;6dB
    Communication Interface USB/RS232
    Probe interface BNC/LEMO

     

    Company Information:

    KUT-681 Digital Portable Ultrasonic Flaw Detector, for metal weld crack, inclusion, pore defect inspection & composite thickness testing

    Contact Details
    Guangdong Hongtuo Instrument Technology Co,Ltd

    Contact Person: Mr. zhong

    Tel: +8613267004347

    Fax: 86-769-23181253

    Send your inquiry directly to us (0 / 3000)

    Other Products